EPAMOULD 745 D 35

EPAMOULD 745 D 35 is a polyether based thermoplastic polyurethane, with excellent physical and mechanical properties, flexibility at low temperature, good transparency, high crystallisation rate and superior resistance to hydrolysis and microbial attack
We recommend using EPAMOULD 745 D 35 for injection molding processes, such as production of technical parts. .


PropertyNormValueUnit
DensityISO 1183-11. 15g/cm³
Hardness (5 sec.)ISO 761946Shore D
Tensile stress at 50% elongationEN 527-1
11.0
MPa
psi
Tensile stress at 100% elongationEN 527-1
12.5
MPa
psi
Tensile stress at 300% elongationEN 527-1
21.6
MPa
psi
Tensile strengthEN 527-1
42
MPa
psi
Elongation @ breakEN 527-1
450
%
%
Tear strengthISO 34-1; B
135
N/mm
pli
AbrasionISO 464950mm³
MFI rate 210°C / 5 kgISO 113310g/10min

Values shown are based on testing of laboratory test specimens, conditioned at 70°C for 14 hours, and represent data that fall within the standard range of properties for the natural material. They are not intended for use in establishing maxiumum, minimum or range of values for specification purpose.

Material preparation

EPAMOULD 745 D 35 is hygroscopic and therefore has to be dried before use. The recommended drying conditions are 2-3 hours at 100 - 110°C in a desiccant dryer. 